MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Tra-Con Tra-Sheet BFGA Thermally Conductive Sheet
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Silicone

Material Notes: TRA-SHEET BFGA is a thermally conductive and insulated silicone sheet with glass fiber reinforcement. It is suitable for heat dissipation applications for high power devices. This product will provide superior thermal performance. Typical applications include providing maximum heat transfer between an active device and a heat spreader or heat sink.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/cc
Thickness 300 microns11.8 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8888
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.90e+15 ohm-cm7.90e+15 ohm-cm
Dielectric Constant 3.33.3
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 5.00 W/m-K34.7 BTU-in/hr-ft²-°F
Flammability, UL94 V-0V-0
 
Descriptive Properties
Color White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 399 X 91042 Polycarbonate (PC), Thermally Conductive - Electrically Insulative
Overview of materials for Vinyl Ester Sheet Molding Compound
Celanese CoolPoly® D5108 Thermally Conductive Polyphenylene Sulfide

PTRAC217 / 71145

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.