System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical DOP Plasticizer
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
Material Notes:
Applications: Leather, Sheet, Cable, Gloves, Hoses, Footwear, Wallpaper
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Viscosity
54
cP
54
cP
Molecular Weight
391
g/mol
391
g/mol
Chemical Properties
Metric
English
Comments
Acid Value
<= 0.070
@Treatment Temp. 125 °C,
Time 10800 sec
<= 0.070
@Treatment Temp. 257 °F,
Time 3.00 hour
After Heating, KOH mg/g; JIS K6751
Thermal Properties
Metric
English
Comments
Melting Point
-55.0
°C
-67.0
°F
Freezing Point
Boiling Point
386
°C
727
°F
Flash Point
206
°C
403
°F
Descriptive Properties
Acidity
<0.02 KOH mg/g
JIS K6751
Color
<20 APHA
JIS K6751
Ester Value
285-289
JIS K6751
Heat Loss
<0.07%
125°Cx3hr, JIS K6751
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LG Chemical EM500 Impact modifier for Engineering Plastics
LG Chemical EM500A Impact modifier for Engineering Plastics
LG Chemical HIPS MI750L PS, Impact Modified
LG Chemical DIDP Plasticizer
LG Chemical HIPS MI750 PS, Impact Modified
PLAY248 / 148258
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.