Notes: Monprene CP-18160 is a high performance thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-18160 is a medium hardness grade suitable for injection molding. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: General Purpose; Good Colorability; Good Moldability; High Elongation; High Flow; Low Density; Low Specific Gravity; Slip; Medium Hardness; Without Fillers Uses: Consumer Applications; Gaskets; Handles; Kitchenware RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |