MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ChevronTexaco Pinnacle® EP 1000
Categories: Fluid; Lubricant

Material Notes: Texaco Pinnacle EP oils deliver value through:
  • Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longer lubricant and equipment life.
  • High viscosity index and low pour point — These result in very broad operating temperature ranges -46°C to 149°C (-50°F to 300°F) when compared with conventional mineral oil based lubricants.
  • Energy savings — The synthetic base oil will typically increase gear efficiency, resulting in less power consumption.
  • Extended drain intervals — Longer lubricant life, reduced maintenance costs, and less used oil disposal when compared to mineral oil products.

Texaco Pinnacle EP oils are high quality industrial EP gear lubricants.

They provide excellent load carrying and antiwear properties; protection against rust, corrosion, foaming, and oxidation; and excellent demulsibility resulting in high performance in most types of industrial gearboxes, exemplified by the FZG pass stage of >12.

These products possess very high shear stability even under heavily loaded, high speed conditions in industrial gears.

The low pour point and very good low temperature fluidity of Texaco Pinnacle EP oils impart improved lubrication during startup at sub-zero temperatures.

Their superior viscosity-temperature characteristics provide dependable lubrication at high temperatures.

A unique property of the synthetic base oil is a low traction coefficient, resulting in improved gear efficiency, energy savings, less friction, less wear, and lower operating temperatures compared to conventional mineral oil products.

Due to the very high viscosity index, these products provide a much higher oil viscosity at operating temperature than a mineral oil product of the same ISO grade. This results in increased oil film thickness and better antiwear protection for both bearings and gears.

Texaco Pinnacle EP oils are recommended for all types of enclosed industrial gearboxes:

  • Especially those running continuously at temperatures up to 107°C(225°F)
  • Or exposed to very cold temperatures as low as -46°C(-50°F)
  • Or under severe service conditions, such as heavy loads or low speeds.

These products also provide excellent protection for bearings operating under similar conditions.

They can be problem-solvers for applications where mineral oil products deteriorate too rapidly or lead to premature failures.

Texaco Pinnacle EP oils meet the requirements of:

  • U.S. Steel 224
  • AGMA 9005 and qualify as AGMA EP gear lubricants

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222076; MSDS Number: 8611

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 32.5 °32.5 °
Viscosity Measurement 162162Viscosity Index
Saybolt Viscosity at 100°F 4984.4 SUS4984.4 SUS
Saybolt Viscosity at 210°F 384.5 SUS384.5 SUS
Kinematic Viscosity at 40°C (104°F) 950 cSt950 cSt
Kinematic Viscosity at 100°C (212°F) 79.65 cSt79.65 cSt
 
Mechanical PropertiesMetricEnglishComments
Timken Test 38500 g85.0 lbOK Load
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -45.6 °C-50.0 °F
Pour Point -30.0 °C-22.0 °F
Flash Point 258 °C496 °F
 
Descriptive Properties
AGMA Grade8A
FZG Pass Stagemin 12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pinnacle Polymers 1120 H Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat
Pinnacle Polymers 2135 Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 2135 H Medium Impact Polypropylene Copolymer, Injection Molding Grade
Pinnacle Polymers 1402 C Clarified Polypropylene Homopolymer Thermoforming Grade
Pinnacle Polymers 1335 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat

WTEXA127 / 77006

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.