MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Graft Polymer GRAFTABOND™ SB-GMA 00330 C Styrene Butadiene Copolymer Grafted with Glycidyl Methacrylate
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: GRAFTABOND™ SB-GMA 00330 C is a copolymer of styrene and butadiene, grafted with high glycidyl methacrylate content. This product provides enhanced stiffness and toughness to materials, while also maintaining excellent compatibility with polar and non-polar polymers, fibers and fillers.

Applications:

  • GRAFTABOND™ SB-GMA 00330 C is a great additive for increasing toughness of rigid materials
  • Excellent compatibility with many polymers and polymer compounds.
Supplied as: Granulate.

Properties can be regulated to customer needs.

Information provided by Graft Polymer LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 2.0 - 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Descriptive Properties
Drying Loss<0.5 g/cc. ASTM D6980
Glycidyl Methacrylate Graft Level2.5 to 3%, FTIR Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Graft Polymer GRAFTABOND™ PPC-GMA 02030 C Polypropylene grafted with Glycidyl Methacrylate
Graft Polymer GRAFTABOND™ PO-SAN 00647 IM Polyethylene Octene, grafted with Styrene Acrylonitrile
Graft Polymer GRAFTABOND™ SB-MAH 00220 C Styrene Butadiene Copolymer Grafted with Maleic Anhydride
Graft Polymer GRAFTABOND™ SB-MAH 03020 C Styrene Butadiene Copolymer Grafted with Maleic Anhydride
Graft Polymer GRAFTABOND™ SAN-MAH 01530 C Styrene Acrylonitrile Copolymer Grafted with Maleic Anhydride

PGRAFT911 / 232342

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.