MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Haysite Dura-Core 1000B Balsa Core Composite Panel
Categories: Polymer; Wood and Natural Products

Material Notes: Balsa-core composite laminate engineered for use as a floor material in light transit rail car interiors.

Information provided by Haysite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.123 g/cc0.00446 lb/in³Core; ASTM D1622
 0.459 g/cc0.0166 lb/in³Composite; ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 5757Composite; ASTM D2583
Tensile Strength 4.72 MPa684 psiComposite Flatwise; ASTM C297
Compressive Strength 7.87 MPa1140 psiComposite Flatwise; ASTM C365
 12.9 MPa1880 psiCore; ASTM D1621
Shear Modulus 0.175 GPa25.4 ksiComposite; ASTM C273
Shear Strength 2.30 MPa333 psiComposite Flatwise; ASTM C273
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
 
Descriptive Properties
Radiant Panel - Flame Spread32.95ASTM E162
Smoke and ToxicityCarbon Monoxide100 ppm, Passes BSS 7239
 Hydrogen Chloride0.8 ppm, Passes BSS 7239
 Hydrogen Cyanide1.5 ppm, Passes BSS7 239
 Hydrogen Fluoride0 ppm, Passes BSS 7239
 Nitrogen Dioxide1.0 ppm, Passes BSS 7239
 Sulfur Dioxide0 ppm, Passes BSS 7239
Smoke Density, 4.0- Minutes Flaming12.7ASTM E662 Optical Density
Smoke Density, 4.0- Minutes Non-Flaming3.4ASTM E662 Optical Density

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHAY517j / 238966

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.