Description: AKROMID C3 GF 30 1 black (4401) is a 30% glass fiber reinforced, heat stabilized polyamide 6.6/6 – Blend. Applications are mainly components in mechanical engineering and the automotive industry where good flowability is required. Additive: Heat Stabilizer Features: Uses:- Automotive Applications
- Engineering Parts
Information provided by Akro-Plastic GmbH |