MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Copper-flo™ No. 3 Copper-Phosphorus Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: Copper-flo™ No.3 is a copper-phosphorus brazing filler metal containing a nominal 6.2% phosphorus and conforming to EN 1044 1999 CP203. It is primarily used for the brazing of copper tubes and pipes in refrigeration and air-conditioning applications and is a popular choice for this type of work.

When it is used to braze copper the phosphorus within the alloy imparts a metallurgical based self-fluxing capability. If used to join copper alloys (such as brass, bronze or gun metal) a separate flux will be required because the self-fluxing action only occurs on copper.

This filler metal should not be used to braze iron containing materials like carbon or stainless steels or nickel containing materials as the phosphorus within the filler metal will form brittle, inter-metallic, phosphide compounds at the joint interface. Copper-flo™No.3 is not suitable for use in joints exposed to sulfurous atmospheres at elevated service temperatures.

When selecting a copper-phosphorus brazing filler metal it is necessary to understand about their flow properties and ductility. The level of phosphorus within the filler metal controls these two characteristics - the higher this is the more free flowing the filler metal and the lower its ductility.

Copper-flo™No.3 due to its lower phosphorus content is less free flowing and slightly more ductile than Copper-flo™. It has a long melting range and a tendency to liquate. This property can be used to aid bridging of comparatively wide joint gaps. Copper-flo™No.3 is suited for joint clearances of 0.75-0.2 mm.

Copper-flo™No.3 is widely used for brazing copper pipes, tubes and fittings in the refrigeration, heating and ventilating and air conditioning systems.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 714 - 890 °C
Solidus 714 °C
Liquidus 890 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 93.8 %
Phosphorus, P 6.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High-Leaded Tin Bronze, UNS C93600, Centrifugal Cast M02
Gray Cast Iron, ASTM A 48 Class 40
High-Leaded Tin Bronze, UNS C93800, Copper Casting Alloy, Centrifugally Cast
Leaded Red Brass, UNS C83600, Copper Casting Alloy (Bronze SAE 40)
MetalTek MTEK 85-5-5-5 Cast UNS C83600 Bearing Bronze

NJMMJ9726 / 186127

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.