MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Extrusion 87262 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: The Cell Classification was determined using the notched Izod test with injection molded samples.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 8015 sec; ASTM D2240
Tensile Strength, Yield 40.9 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2610 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 73.0 MPaASTM D790
Flexural Modulus 2520 MPaASTM D790
Izod Impact, Notched 810 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Compression Molded, Flow; ASTM D256A
 1100 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Compression Molded, Across Flow; ASTM D256A
Dart Drop Total Energy 36.0 J/cm
@Temperature 23.0 °C
Procedure A, C.125; ASTM D4226
 36.0 J/cm
@Temperature 23.0 °C
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.749 mm
ALL; UL 94
 5VA
@Thickness 3.00 mm
ALL; UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 193 °C
 
Descriptive Properties
Agency RatingsNSF 51
Ease of SizingExcellent
FeaturesGood Dimensional Stability
 Good Melt Strength
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification16244ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesProfiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Flexible C7000 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Flexible 82024 Polyvinyl Chloride, Flexible

PH0POL0017 / 144586

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.