MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
UBE UPISEL-N BE1210 Copper Clad Laminate
Categories: Metal; Polymer

Material Notes: Description: UPISEL-N BE1210 is non-adhesive type flexible Copper Clad Laminate (Polyimide = 25µm, Cu = 18µm) based on "UPILEX-VT." UPISEL-N has excellent dimensional stability and heat resistance. "UPILEX-VT" performs high bonding ability without any use of adhesives by simple heat lamination. "UPILEX-VT" is an aromatic polyimide same as "UPILEX-S" which has high market share as the base film for TAB (Tape Automated Bonding).

Applications:

  • FPC
  • TCP
  • MCM-L
  • COF
  • Rigid flex
  • Multi-layer boards
  • Metal based boards
  • High frequency boards
  • Heat-resistant boards
  • IC cards
  • Boards for automobile
  • Electromagnetic wave shield material
  • HDD suspension

Characteristics:

  • Without the use of adhesives, UPISEL-N maintains high physical properties and high reliability at high temperatures
  • It performs excellent peeling strength, heat soldering resistance, chemical resistance and dimensional stability
  • The film layer of the UPISEL-N can be heat bonded with ceramics, metals and silicon chip
  • Without the use of adhesives, UPISEL-N is tender for the environment

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 1.0 %IPCTM 650
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 54 %ASTM D882
Tensile Modulus 68000 kg(f)/cm²ASTM D882
Peel Strength 0.686 kN/mT Peel (Width=10), 300°C; IPC-FC-241B
 1.08 kN/m90° Peel (Width=10) after 200°C for 7 days; IPC-FC-241B
 1.08 kN/m90° Peel (Width=3.2), 100% Retained with 2N-HCl or 2N-NaOH; IPC-FC-241B
 1.275 kN/mT Peel (Width=10), 250°C; IPC-FC-241B
 1.37 kN/mT Peel (Width=10), 25°C; IPC-FC-241B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 5.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohmASTM D257
Dielectric Constant 3.2
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0023
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0VTM-0
Shrinkage 0.025 %After Cu Etching; IPC-FC-241B
 0.060 %After Cu Etching; IPC-FC-241B
 0.035 %
@Temperature 150 °C,
Time 1800 sec
IPC-FC-241B
 0.080 %
@Temperature 150 °C,
Time 1800 sec
IPC-FC-241B
 
Descriptive Properties
Flexural Endurance (MD)110,000 cyclesIPC-FC-241B
Flexural Endurance (TD)150,000 cyclesIPC-FC-241B
Folding Endurance RO.4 (MD)48 cyclesJPCA FC01
Folding Endurance RO.4 (TD)48 cyclesJPCA FC01
Hot Solder Resistance: 300°C 1 min.No ChangeIPC-FC-241B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Aluminum Alloy
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48
Limestone
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative
Overview of materials for Copper Alloy

PUBE241 / 71799

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.