MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aclo Accucomp Polyethylene LD0109L Low Density
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D792
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inMD; ASTM D955
Melt Flow 50 g/10 min50 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 4040ASTM D785
Tensile Strength at Break 8.00 MPa1160 psiASTM D638
Tensile Strength, Yield 10.0 MPa1450 psiASTM D638
Elongation at Break 112 %112 %ASTM D638
Elongation at Yield 27 %27 %ASTM D638
Tensile Modulus 0.320 GPa46.4 ksiASTM D638
Flexural Strength 9.03 MPa1310 psiASTM D790
Flexural Modulus 0.300 GPa43.5 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 °C113 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Medium Density Polyethylene (MDPE), Molded
Aclo Accucomp Polyethylene LD0102L Low Density
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Overview of materials for Medium Density Polyethylene (MDPE), Extruded

PACLO073 / 22328

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.