MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast & Aged)
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Pouring Temperature: 1095-1175°C
Heat treatment required for max strength (Annealing): 870-900°C/water quench
Heat treatment required for max strength (Hardening): 870-900°C/water quench

Description: The unique combination of physical and mechanical properties of copper beryllium casting alloys provide a dynamic range of metallurgical alternatives to meet specific performance requirements. The inherent strength, hardness, conductivity, and castability of these materials make them ideal for applications which require a high performance engineered material solution. Advancements in component casting technology and proprietary material production technology pioneered by Brush Wellman have resulted in BrushCAST™ alloys being a cost effective design choice.

Alloy 3C offers excellent electrical and thermal conductivity, good strength & galling resistance, and accurate replication of component detail. Alloy 3C offers nearly 3 times the conductivity of the high strength alloys, twice the thermal conductivity of aluminum alloys, and ten times that of steel.

Information supplied by Brush Wellman Engineered Materials.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: UNS C82200
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 75 - 9075 - 90
Tensile Strength, Ultimate 414 - 517 MPa60000 - 75000 psi
Tensile Strength, Yield 276 - 379 MPa
@Strain 0.2 %
40000 - 55000 psi
@Strain 0.2 %
Elongation at Break 10 - 20 %10 - 20 %
Modulus of Elasticity 138 GPa20000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000344 - 0.00000382 ohm-cm0.00000344 - 0.00000382 ohm-cmConductivity is 45-50% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 21.1 - 204 °C
10.0 µin/in-°F
@Temperature 70.0 - 400 °F
Thermal Conductivity 249.0 W/m-K1728 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.35 - 0.80 %0.35 - 0.80 %
Copper, Cu 98 %98 %as balance
Nickel, Ni 1.0 - 2.0 %1.0 - 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBBC23 / 15333

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.