MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elmet-Starck 3402 Molybdenum Alloy AST-4 TZM, Arc-Cast Sheet
Categories: Metal; Nonferrous Metal; Molybdenum Alloy

Material Notes: Arc-Cast Sheet 3402

Description of Product: This specification covers rolled sheet of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated by the H.C. Stark consumable electrode vacuum-arc-casting process.

Structure: Plate will be supplied in a stress-relieved condition unless otherwise requested.

Information provided by H.C. Starck.

Elmet Technologies Acquired H.C. Starck Solutions Americas in 2023.

Vendors: Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  >= 827 MPa
@Thickness 0.254 - 0.635 mm
>= 120000 psi
@Thickness 0.0100 - 0.0250 in
ASTM E-8
 >= 827 MPa
@Thickness 0.635 - 1.52 mm
>= 120000 psi
@Thickness 0.0250 - 0.0600 in
ASTM E-8
 >= 827 MPa
@Thickness 1.52 - 2.29 mm
>= 120000 psi
@Thickness 0.0600 - 0.0900 in
ASTM E-8
 >= 827 MPa
@Thickness 2.29 - 4.75 mm
>= 120000 psi
@Thickness 0.0900 - 0.187 in
ASTM E-8
Tensile Strength, Yield  >= 689 MPa
@Strain 0.2 %,
Thickness 0.254 - 0.635 mm
>= 100000 psi
@Strain 0.2 %,
Thickness 0.0100 - 0.0250 in
ASTM E-8
 >= 689 MPa
@Strain 0.2 %,
Thickness 0.635 - 1.52 mm
>= 100000 psi
@Strain 0.2 %,
Thickness 0.0250 - 0.0600 in
ASTM E-8
 >= 689 MPa
@Strain 0.2 %,
Thickness 1.52 - 2.29 mm
>= 100000 psi
@Strain 0.2 %,
Thickness 0.0600 - 0.0900 in
ASTM E-8
 >= 689 MPa
@Strain 0.2 %,
Thickness 2.29 - 4.75 mm
>= 100000 psi
@Strain 0.2 %,
Thickness 0.0900 - 0.187 in
ASTM E-8
Elongation at Break  >= 6.0 %
@Thickness 0.254 - 0.635 mm
>= 6.0 %
@Thickness 0.0100 - 0.0250 in
ASTM E-8
 >= 7.0 %
@Thickness 0.635 - 1.52 mm
>= 7.0 %
@Thickness 0.0250 - 0.0600 in
ASTM E-8
 >= 9.0 %
@Thickness 1.52 - 2.29 mm
>= 9.0 %
@Thickness 0.0600 - 0.0900 in
ASTM E-8
 >= 10 %
@Thickness 2.29 - 4.75 mm
>= 10 %
@Thickness 0.0900 - 0.187 in
ASTM E-8
Bend Radius, Minimum 2.0 t
@Thickness <=1.65 mm
2.0 t
@Thickness <=0.0650 in
Bend Severity 90°, specimens at least 1" by 2", transverse direction
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.010 - 0.030 %0.010 - 0.030 %
Iron, Fe <= 0.010 %<= 0.010 %
Molybdenum, Mo >= 99.25 %>= 99.25 %by difference
Nickel, Ni <= 0.0020 %<= 0.0020 %
Nitrogen, N <= 0.0020 %<= 0.0020 %
Oxygen, O <= 0.0030 %<= 0.0030 %
Silicon, Si <= 0.010 %<= 0.010 %
Titanium, Ti 0.40 - 0.55 %0.40 - 0.55 %
Zirconium, Zr 0.060 - 0.12 %0.060 - 0.12 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elmet-Starck 3403 Molybdenum Alloy APT-3 TZM, Arc-Cast Plate
Elmet-Starck Molybdenum Alloy TZM ABT, Arc-Cast Bar
Elmet-Starck 2702 Molybdenum Alloy P/M - TZM Sheet
Plansee TZM sheet
Plansee TZM Titanium-Zirconium-Molybdenum Rod

NHCST904 / 130794

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.