MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Clearway® 3 De-icer
Categories: Other Engineering Material

Material Notes: Product Description: Eastman’s de-icers are marketed under the brand name Clearway®. Clearway is acknowledged as one of the leaders in airport runway de-icing and the product range has been developed and expanded to include both liquid and solid formate-based and acetate-based products. Based on a formulation of potassium acetate and corrosion inhibitors, Clearway 1 has been on the market for nearly 30 years as an effective liquid runway de-icer with low environmental impact. The product meets not only all relevant environmental and ecological requirements but also the AMS 1435 standard. Clearway 1 is classified WGK1* both for its biodegradability and because of its low aquatic toxicity. When applied with the mechanical facilities of airport maintenance departments, Clearway 1 allows snow and ice to be removed quickly and economically. Clearway 1 melts the ice by depressing the freezing point of water. Due to its low freezing point, the resultant solution will have a much lower freezing point.

Application/Uses:

  • Airport runway de-icing

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 - 1.30 g/cc0.0452 - 0.0470 lb/in³
Viscosity  12 - 20 cP
@Temperature 20.0 °C
12 - 20 cP
@Temperature 68.0 °F
 65 - 85 cP
@Temperature -10.0 °C
65 - 85 cP
@Temperature 14.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point <= -50.0 °C<= -58.0 °FFreezing Point
 -17.0 °C1.40 °FFreezing Point; fluid diluted 1:1
 
Descriptive Properties
AppearanceClear to slightly hazy liquid
Content>50%Assay, active material

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5094 / 222288

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.