Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber, 33% Filler by Weight Additive: Heat Stabilizer and PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance, Heat Stabilized and Low Friction Information provided by TP Composites, Inc. |