MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Apec® RW1697 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: MVR (330 °C/2.16 kg) 45 cm³/10 min; easy release; low viscosity; softening temperature (VST/B 120) = 157°C

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption at Equilibrium 0.12 %ISO 62
Water Absorption at Saturation 0.30 %ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm60 x 60 x 2 mm3; 500 bar holding pressure; ISO 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm60 x 60 x 2 mm3; 500 bar holding pressure; ISO 2577
Melt Flow 45 g/10 min
@Load 2.16 kg,
Temperature 330 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 68.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break 50 %50 mm/min; ISO 527-1,-2
Elongation at Yield 6.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2500 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 110 MPa5 mm/min; ISO 178
Flexural Modulus 2500 MPa2 mm/min; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
acc. ISO 179/1eA
 9.00 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
acc. ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ASTM E831
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 149 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 137 °CISO 75-1,-2
Vicat Softening Point 157 °C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94 HB
@Thickness 3.00 mm
 V-2
@Thickness 1.50 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 95 %
@Thickness 3.00 mm
ISO 5036-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 330 °CInjection; ISO 294
Mold Temperature 100 °CInjection; ISO 294
Injection Velocity 200 mm/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm PLEXIGLAS® XT Clear 0A070 UV transmitting PMMA
Zeon Specialty Materials ZEONEX® 790R Cyclo Olefin Polymer
Covestro Apec® 1600 Polycarbonate
Covestro Apec® 1605 Polycarbonate
Covestro Makrolon® AU sheet Polycarbonate

PCOVEST0011 / 201794

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.