MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NUDEC® PC Polycarbonate Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: NUDEC® PC polycarbonate plastic sheets are outstanding for their impact strength and high temperature resistance. They are often employed in construction sector applications, such as coatings, coverings and anti-vandal town furniture. Available with with a pattern and/or opaque colors, to be applied in the automotive industry, either as part of the auxiliary assembly or even as part of the automobile. Also available is a UV version. These sheets possess special co-extruded UV protection that permits them to be used in outside applications in which they are exposed to UV light.

Information provided by NUDEC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 72ASTM D-785
Hardness, Rockwell R 118ASTM D-785
Tensile Strength at Break 72.0 MPaISO 527
Tensile Strength, Yield 60.0 MPaISO 527
Elongation at Break >= 150 %ISO 527
Tensile Modulus 2.30 GPaISO 527
Flexural Strength 97.0 MPaISO 178
Izod Impact, Notched 950 J/m
@Temperature 23.0 °C
ISO 180
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ISO 180
Charpy Impact, Notched 55.0 kJ/m²
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear >= 68.0 µm/m-°CASTM D-696
Maximum Service Temperature, Air 120 °C
Deflection Temperature at 0.46 MPa (66 psi) 146 °CHDT B; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 143 °CHDT A; ISO 75-2
Vicat Softening Point 151 °C
@Load 5.10 kg
ISO 306B
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D-542
Transmission, Visible 87 - 91 %ASTM D-1003
 
Descriptive Properties
Chemical ResistanceAcetic Acidsatisfactory
 Acetoneunsatisfactory
 Ammoniaunsatisfactory
 Detergentssatisfactory
 Ethanolsatisfactory
 Gasolineunsatisfactory
 Glycerinregular
 Methanolunsatisfactory
 Mineral oilsatisfactory
 Tolueneunsatisfactory
 Turpentineunsatisfactory
 vegetable oilsatisfactory
 Watersatisfactory
FlammabilityFrance, NFP 92-507, M2
 Germany, DIN 4102-1, B1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Cyrolon® AR Polycarbonate Sheet
Spartech UltraTuf SG Polycarbonate Sheet
Evonik EUROPLEX® SDX Polycarbonate Sheet
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced

PNUDEC993 / 192059

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.