MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Redwood Plastics Redco™ ACETAL COPOLYMER
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Redco™ Acetal brings together the benefits of strength, stiffness, a low coefficient of friction, and dimensional stability providing a versatile and easily machinable material that exceeds the life of many parts that are traditionally metal. Suited for a variety of industries and applications, Redco™ Acetal acts as an electrical insulator, is FDA Approved for food applications, and is an excellent material for use in applications requiring close-tolerances. To minimize delivery times and meet design configurations, Redwood Plastics and Rubber stocks a broad array of Redco™ Acetal sheet and round bar in both white and black. Custom colors and sizes are also available upon request.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
Water Absorption 0.22 %
@Thickness 3.17 mm,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80At 0.2 in/min loading rate; ASTM D785
Tensile Strength 5000 psi
@Temperature >=71.1 °C
ASTM D638
 8800 psi
@Temperature >=22.8 °C,
Time 86400 sec
ASTM D638
Elongation at Break 55 %ASTM D638
Tensile Modulus 400000 psiASTM D638
Flexural Strength 13000 psiASTM D790
Flexural Modulus 400000 psiASTM D790
Compressive Strength 15000 psiASTM D695
Compressive Modulus 400000 psiASTM D695
Fatigue Strength 3300 psi
@# of Cycles 1.00e+7
ASTM D671
Shear Strength 8000 psiASTM D732
Izod Impact, Notched 1.30 ft-lb/inASTM D256
 20.0 ft-lb/inASTM D256
Coefficient of Friction 0.15VS. STEEL
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm50% RH; ASTM D257
Dielectric Constant 3.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 500 V/mil
@Thickness 2.29 mm
short time; ASTM D149
 2100 V/mil
@Thickness 0.127 mm
short time; ASTM D149
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 240 sec
@Thickness 3.05 mm
burns; ASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 85.0 µm/m-°C
@Temperature -40.0 - 185 °C
ASTM D696
Thermal Conductivity 1.60 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 180 °F
Deflection Temperature at 0.46 MPa (66 psi) 316 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °CASTM D648
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW042 / 296608

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.