MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF 1,4-Butanediol (BDO)
Categories: Fluid

Material Notes: Formula: C4H10N2

CAS: 110-63-4

Description: 1,4-Butanediol (BDO) is a colorless, odorless liquid. It is miscible in all proportions with water and soluble with organic solvent.

Synonyms: Butane-1,4-diol

Applications: Intermediate used in the production of Initial product for chemical syntheses, Paint industry and Plastics industry

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.0169 g/cc
Molecular Weight 90.1 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 20.0 °C
Boiling Point 166 °C
Flash Point 134 °C
Ignition Temperature 385 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.050 %DIN 51 777
 
Descriptive Properties
Assay>99.5%
Color<10APHA 8415

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Boric Acid (orthoboric acid), B(OH)3
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 73A Polyurethane, MDI PPG
Polikim ULPOLEN® 1000 UHMWPE, Oil
Covestro DESMODUR® MAX-TD0410-7 + MOCA Polyurethane, MDI-PTMEG
Covestro DESMODUR® LU-D80 + MOCA Polyurethane, TDI-Ester

PBASG0874 / 132507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.