MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Monprene® RG-17260 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-17200 series is a group of high performance thermoplastic elastomers specifically designed for EU injection molded regulated applications including food contact, toys, and children’s products. Monprene RG-17260 is a medium density, medium hardness grade that complies with various US FDA and European regulations and directive for food contact and toy safety and is suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; Medium Density; Medium Hardness; Lubricated

Uses: Closures; Consumer Applications; Cosmetic Packaging; Gaskets; Handles; Kitchenware; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Viscosity 109 cP
@Shear Rate 206 1/s,
Temperature 200 °C
109 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ISO 11443
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60
@Time 5.00 sec
60
@Time 0.00139 hour
ISO 868
Tensile Strength at Break 8.00 MPa1160 psiISO 37
Tensile Stress at Strain  2.00 MPa
@Strain 100 %
290 psi
@Strain 100 %
ISO 37
 2.10 MPa
@Strain 300 %
305 psi
@Strain 300 %
ISO 37
Elongation at Break 800 %800 %ISO 37
Compression Set  26 %
@Temperature 22.8 °C,
Time 79200 sec
26 %
@Temperature 73.0 °F,
Time 22.0 hour
Method B; ISO 815
 47 %
@Temperature 70.0 °C,
Time 79200 sec
47 %
@Temperature 158 °F,
Time 22.0 hour
Method B; ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 120 - 160 °C248 - 320 °F
Middle Barrel Temperature 160 - 230 °C320 - 446 °F
Front Barrel Temperature 180 - 230 °C356 - 446 °F
Nozzle Temperature 180 - 230 °C356 - 446 °F
Melt Temperature 180 - 230 °C356 - 446 °F
Mold Temperature 15.0 - 50.0 °C59.0 - 122 °F
Back Pressure 0.500 - 1.50 MPa72.5 - 218 psi
Cushion 0.300 - 2.00 cm0.118 - 0.787 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0928 / 237419

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.