MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company EMI 1061 Polybutylene Terephthalate (PBT), Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polyester, Steel Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D 792
Additive Loading 10 %Primary Additive
Linear Mold Shrinkage 0.012 - 0.016 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8200 psiASTM D 638
Elongation at Break >= 10 %ASTM D 638
Tensile Modulus 450 ksiASTM D 638
Flexural Strength 13600 psiASTM D 790
Flexural Modulus 450 ksiASTM D 790
Izod Impact, Notched 0.700 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 11.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.0 ohm-cmASTM D 257
Surface Resistance <= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Shielding Effectiveness 49 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 49 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 49 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 50 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 50 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 51 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 125 °FASTM D 648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 430 °F
Mold Temperature 145 - 180 °F
Drying Temperature 250 °F
@Time 14400 sec
Moisture Content 0.030 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company EMI 1363 Polyphenylene Sulfide (PPS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1361 Polyphenylene Sulfide (PPS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 1062 Polybutylene Terephthalate (PBT), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection

PQZWA2912 / 91419

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.