MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 200 TC-C-30 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant - Preliminary Datasheet
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Preliminary Data Sheet

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.65 g/cc1.65 g/ccASTM D 792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.17 mm
0.0010 - 0.0030 in/in
@Thickness 0.125 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 68.9 MPa10000 psiASTM D 638
Elongation at Break 1.0 - 2.0 %1.0 - 2.0 %ASTM D 638
Tensile Modulus 15.9 GPa2300 ksiASTM D 638
Flexural Strength 103 MPa15000 psiASTM D 790
Flexural Modulus 15.2 GPa2200 ksiASTM D 790
Izod Impact, Notched 0.267 J/cm
@Thickness 3.17 mm
0.500 ft-lb/in
@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 1.60 J/cm
@Thickness 3.17 mm
3.00 ft-lb/in
@Thickness 0.125 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 100 ohm-cm<= 100 ohm-cmASTM D 257
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.29 W/m-K15.9 BTU-in/hr-ft²-°FThrough-plane; ASTM E 1530
 14.0 W/m-K97.2 BTU-in/hr-ft²-°FIn-plane; ASTM E 1461-92
Deflection Temperature at 1.8 MPa (264 psi) 238 °C460 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 299 °C530 - 570 °F
Mold Temperature 65.6 - 107 °C150 - 225 °F
Drying Temperature 79.4 °C
@Time 14400 sec
175 °F
@Time 4.00 hour
Moisture Content 0.20 %0.20 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 124 MPa10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 299 X 124222 B Nylon 6/6 (PA); Thermally Conductive - Electrically Conductive - Flame Retardant - Preliminary
RTP Company RTP 200 TC-C-40 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant
Avient Therma-Tech™ NNC-5000 TC Polyamide 66 (Nylon 66)
RTP Company RTP 1399 X 128637 B Polyphenylene Sulfide (PPS), Thermally Conductive - Electrically Conductive
Avient Therma-Tech™ NJC-6000 TC Nylon 12

PQZTA21589 / 159145

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.