MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Trigonox 75 Methyl ethyl ketone peroxide
Categories: Other Engineering Material

Material Notes: Trigonox 75 is a peroxide mixture, specially developed for the production and cure of thick laminates and for applications where a high peak exotherm should be avoided. Application: pipes, tanks, windmill rotors.

CAS number: 1338-23-4

EINECS/ELINCS No: 215-661-2

Applications: Trigonox 75 is a methyl ethyl ketone peroxide formulation for the curing of unsaturated polyester resins in the presence of a cobalt accelerator at room and elevated temperatures. In thin laminates up to approx. 4 mm Trigonox 75 performs comparable with Butanox M-50, however, in thicker laminates up to approx. 10 mm Trigonox 75 gives a reduced peak exotherm at equal gel time and curing time. Therefore, Trigonox 75 is suitable for the cure of both thin and thick sections in one particular product.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
Viscosity 20 cP
Storage Temperature <= 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 60.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Content3.1-3.5 %tert-Butyl hydroperoxide
 9.8-10.0 %Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY1139 / 286662

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.