MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond UV15X-6Med-2LV UV system for high performance bonding, sealing and coating
Categories: Polymer; Thermoset

Material Notes: Master Bond UV15X-6Med-2LV is a one component, medium viscosity UV system featuring high flexibility, excellent toughness and superior abrasion resistance. It can be used for a wide variety of applications including bonding, sealing, coating and encapsulation. Its robust flexibility allows it to withstand severe thermal cycling as well as resisting thermal and mechanical shocks. UV15X-6Med- 2LV bonds well to a variety of substrates, especially glass, polycarbonates and acrylics as well as many other plastics, metals and rubbers. It has good chemical resistance to water, cleaning agents, chemical sterilants, EtO and gamma radiation. UV15X-6Med-2LV is a top notch thermal and electrical insulator with a service temperature range of -80°F to +250°F. UV15X-6Med-2LV generally cures readily in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the system’s distance from the light source, the thickness of the section and of course the intensity of the light source. It should be noted that the system can cure in sections approaching 1/4 inch thick. However, when bonding, sections of a few thousandths of an inch are more than adequate. Most importantly, UV15X-6Med-2LV does not display oxygen inhibition. This system is widely used in medical device manufacturing and specialty applications where ISO 10993-5 requirements are desirable.

Product Advantages:

  • One part system with no mixing needed
  • Cures fast upon exposure to 320-365 nm UV light at ambient temperatures. No oxygen inhibition
  • Outstanding toughness and abrasion resistance
  • Withstands rigorous thermal cycling
  • Passes ISO 10993-5 for cytotoxicity
Key Features:
  • Superior abrasion resistance
  • Meets ISO 10993-5
  • High flexibility and toughness
  • Moderate viscosity

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
Viscosity 20000 - 40000 cP20000 - 40000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 6555 - 65
Tensile Strength 6.89 - 11.0 MPa1000 - 1600 psi
Elongation at Break >= 100 %>= 100 %
Tensile Modulus 0.138 - 0.345 GPa20.0 - 50.0 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cm
Dielectric Constant 4.5
@Frequency 60 Hz
4.5
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -62.0 °C-79.6 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.501.50
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM645 / 268833

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.