MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akroloy® PA LGF 50 natural (5504) PA 6.6 + PA 6I/6T, 50% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: LGF. Long fiber, high notched impact strength. PA 6.6 + PA 6I/6T LGF 50.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³ISO 1183
Filler Content 50 %50 %ISO 1172
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 260 MPa37700 psi5 mm/min. Conditioned; ISO 527-2
 300 MPa43500 psi5 mm/min. Dry as Molded; ISO 527-2
Elongation at Break 2.3 %2.3 %5 mm/min. Conditioned; ISO 527-2
 2.3 %2.3 %5 mm/min. Dry as Molded; ISO 527-2
Tensile Modulus 18.0 GPa2610 ksi1 mm/min. Conditioned; ISO 527-2
 18.5 GPa2680 ksi1 mm/min. Dry as Molded.; ISO 527-2
Flexural Strength 445 MPa64500 psiDry as Molded. 2 mm/min; ISO 178
Flexural Modulus 18.5 GPa2680 ksi2 mm/min. Dry as Molded; ISO 178
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
Dry as Molded; ISO 179-1/1eA
 11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
 11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
Charpy Impact, Notched  4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
Dry as Molded; ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °FDry as Molded. DES, 10°C/min; DIN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 230 °C446 °FDry as Molded; ISO 75
Deflection Temperature at 8.0 MPa 200 °C392 °FDry as Molded; ISO 75
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Conditioned
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Dry as Molded
 
Descriptive Properties
Burning Rate<100 mm/minDry as Molded. FMVSS 302. >1 mm thickness
 <100 mm/minConditioned. FMVSS 302. >1 mm thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKRO9911 / 255568

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.