MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene
Categories: Polymer; Thermoplastic; Polymethylpentene (PMP); Polymethylpentene, Molded

Material Notes: This grade is highly recommended for injection molding; also for film and fiber extrusion.

TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics and good high frequency electrical and valuable acoustic/ultrasonic properties. Applications include medical and laboratory apparatus, microwave components and cookware and electronic components.

Information provided by Goodfellow. TPX® is a trademark of Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.833 g/ccASTM D1505
Water Absorption <= 0.010 %ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cmMCI Method 2
Linear Mold Shrinkage, Transverse 0.012 cm/cmMCI Method 2
Melt Flow 21 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
Spiral Flow 51.0 cmMCI Method 1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 87ASTM D785
Tensile Strength 30.0 MPaASTM D638
Tensile Strength, Yield 30.0 MPaASTM D638
Elongation at Break 12 %ASTM D638
Tensile Modulus 1.90 GPaASTM D638
Flexural Strength 44.0 MPaASTM D790
Flexural Modulus 1.60 GPaASTM D790
Izod Impact, Notched 0.200 J/cmASTM D256
Izod Impact, Unnotched (ISO) 9.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.1ASTM D150
Dielectric Strength 65.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 117 µm/m-°CASTM E831
Melting Point 233 °CDSC Peak; JIS K7121
Deflection Temperature at 0.46 MPa (66 psi) 127 °CASTM D648
Vicat Softening Point 174 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46ASTM D542
Haze 0.80 %ASTM D1003
Transmission, Visible 94 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
Overview of materials for Polymethylpentene, Molded
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene
Aclo Accutech Polypropylene Copolymer CP0437C30L1 Calcium Reinforced
Aclo Accuguard Polypropylene CP1467V2CSL Copolymer Flame Retardant Copper Stabilized

PGOODF228 / 135580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.