SMC LS 3000 R33 is a sheet molding compound based on an unsaturated polyester resin, halogen-free, reinforced with glass fibers. This SMC has been developed for general purpose. SMC LS 3000 R33 joint excellent mechanical properties and good fluidity. SMC LS 3000 R33 is formulated according to RoHS, REAC regulation (SVHC) and WEEE European legislation.Information provided by Polynt Composites. |