MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Reynolds Dragon Skin® 10 NV Silicone Rubber Compound
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: Dragon Skin™ 10 NV is a low viscosity, high performance platinum cure silicone rubber that is easy to use and versatile. Mix ratio is 1A:1B by weight or volume, pot life is 15 minutes and cure time is 75 minutes at room temperature. Rubber cures with negligible shrinkage to a Shore 10A. Vacuum degassing is not necessary Color is water white translucent. Cured material is skin safe and certified by an independent laboratory. Dragon Skin™ 10 NV is suitable for making molds of any configuration for casting plasters, wax, low-melt temperature metal alloys, and resins. Dragon Skin™ 10 NV is suitable for special effects applications. Color can be added with Silc Pig™ or Ignite™ color pigments. This rubber can be thickened with Thi-Vex™ thickening agent or softened with SLACKER™ additive.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccASTM D-1475
Viscosity 6000 cPMixed; ASTM D-2393
Linear Mold Shrinkage <= 0.0010 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 10ASTM D-2240
Tensile Strength 400 psiASTM D-412
Elongation at Break 663 %ASTM D-412
100% Modulus 27.0 psiASTM D-412
Tear Strength 90.0 pliDie B; ASTM D-624
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 232 °C
Minimum Service Temperature, Air -53.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 75.0 min
Pot Life 15.0 minASTM D-2471
 
Descriptive Properties
ColorTranslucent
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Specific Volume25.8[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN118 / 296819

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.