Crosslinked silicone adhesive with 2 polyester film release liners. Features: - Resistant to extreme temperatures
- High bond strength
- Chemical resistant
Applications: High performance bonding and other applications involving harsh environments. Bonds well to silicone foam, metals and most plastics including low surface energy substrates. Information provided by Dielectric Polymers. |