MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exxtral™ CMV 205 Performance Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive interior applications in which good surface finish and good UV resistance are required.

Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America

Features:

  • Balanced Stiffness/Toughness
  • Good Dimensional Stability
  • Good Colorability
  • Good Impact Resistance
  • Good Surface Finish
  • Low to No Fogging
Uses:
  • Automotive Applications
  • Automotive Interior Parts
  • Automotive Interior Trim
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2540 psiISO 527-2/50
Tensile Strength, Yield 3190 psiISO 527-2/50
Elongation at Break 21 %ISO 527-2/50
Elongation at Yield 3.0 %ISO 527-2/50
Tensile Modulus 305000 psiSecant; ISO 527-2
Charpy Impact, Notched 1.50 ft-lb/in²
@Temperature 0.000 °C
Complete Break; ISO 179
 2.90 ft-lb/in²
@Temperature 22.8 °C
Complete Break; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 235 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 136 °FISO 75-2/A

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exxtral™ BMT222 Performance Polyolefin
ExxonMobil ExxonMobil™ Performance Polyolefin CMU205 Polypropylene Compound
ExxonMobil Exxtral™ CMU 101 Performance Polyolefin
ExxonMobil Exxtral™ BMU130A Performance Polyolefin
ExxonMobil ExxonMobil™ Performance Polyolefin BMV214 Polypropylene Compound

PEX99360 / 175596

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.