MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals Sclair® 2815 HDPE Injection Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Features: Excellent balance of stiffness and toughness, low odor.

Applications: Margarine and spreads, thin walled containers, frozen food containers.

Data provided by the manufacturer.

Key Words: High Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.954 g/ccASTM D792
Apparent Bulk Density 0.610 g/cc
Melt Flow 67 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow 38.0 cmNOVA Snake Flow Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ASTM D2240
Tensile Strength, Yield 27.0 MPaASTM D638
Flexural Modulus 1.07 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 123 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 170 - 260 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DOWLEX™ IP-90 High Density Polyethylene
Dow DMDA-8980 NT 7 High Density Polyethylene Resin
Dow HDPE 65053N High Density Polyethylene
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding

PEHN1V / 35580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.