MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Duct 916H03 Room Temperature Cure High Conductivity Silver Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-DUCT 916H03 is recommended for electronic bonding and sealing applications that require the combination of high conductivity coupled with good mechanical properties. This two part smooth paste silver-filled epoxy adhesive is solvent free, does not contain any copper, nickel or carbon additives, and develops strong, durable electrically and thermally conducting bonds and seals between many different and dissimilar materials such as metals, ceramics, glass and plastic laminates. TRA-DUCT 916H03 cures at room temperature, and can be used as a "cold-solder" for heat-sensitive components where hot-soldering is impractical. It can also be used for the assembly and repair of electrical modules, printed circuits, wave guides, flat cable and high frequency shields.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 57500 cPMixed (cp #52, 5 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 832 hrs @ 65°C
Adhesive Bond Strength 700 psiLap shear, alum to alum, 2 hrs @ 65°C
 700 psiLap shear, alum to alum, 24 hrs @ 25°C
 1475 psiLap shear, alum to alum, 1 hr @ 110°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00010 ohm-cmcured 1 hr @ 110°C
 0.0010 ohm-cmcured 2 hrs @ 65°C
 0.010 ohm-cmcured 24 hrs @ 25°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 42.0 µm/m-°CBelow Tg
 230 µm/m-°CAbove Tg
Glass Transition Temp, Tg 50.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
 
Descriptive Properties
Color Light YellowHardener
 SilverResin/Mixed/Cured
Thixotropic Index 31 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Duct 916H02 Room Temperature Cure, Conductive Silver Epoxy Adhesive
Tra-Con Tra-Duct 916H01 Electronically Conductive Silver-Filled Epoxy
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Epoxy Technology EPO-TEK® E2101 Electrically Conductive, Silver Epoxy
Abatron 8602-2 A/B Carbon-Filled Electrically Conductive Epoxy Compound

PTRAC188 / 71116

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.