MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polypropylene with 40% Mica Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Mica Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.17 - 1.27 g/ccAverage value: 1.22 g/cc Grade Count:27
Filler Content 35.0 - 40.0 %Average value: 39.4 % Grade Count:9
Water Absorption 0.0300 - 0.0400 %Average value: 0.0367 % Grade Count:3
Linear Mold Shrinkage 0.00400 - 0.0130 cm/cmAverage value: 0.00724 cm/cm Grade Count:26
Melt Flow 2.00 - 17.0 g/10 minAverage value: 9.73 g/10 min Grade Count:20
Ash 40.0 %Average value: 40.0 % Grade Count:9
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 33.0 - 104Average value: 61.8 Grade Count:13
Hardness, Shore D 70.0 - 73.0Average value: 72.0 Grade Count:4
Tensile Strength, Ultimate 14.0 - 40.2 MPaAverage value: 27.1 MPa Grade Count:23
 5.00 - 15.0 MPa
@Temperature 60.0 - 90.0 °C
Average value: 10.0 MPa Grade Count:1
Tensile Strength, Yield 15.0 - 46.9 MPaAverage value: 31.3 MPa Grade Count:14
Elongation at Break 3.00 - 10.0 %Average value: 6.18 % Grade Count:17
 5.00 - 20.0 %
@Temperature 60.0 - 90.0 °C
Average value: 12.5 % Grade Count:1
Elongation at Yield 2.00 - 5.00 %Average value: 2.83 % Grade Count:12
 3.00 - 3.50 %
@Temperature 60.0 - 90.0 °C
Average value: 3.25 % Grade Count:1
Modulus of Elasticity 2.50 - 4.83 GPaAverage value: 3.69 GPa Grade Count:12
 1.20 - 2.50 GPa
@Temperature 60.0 - 90.0 °C
Average value: 1.85 GPa Grade Count:1
Flexural Yield Strength 22.0 - 65.0 MPaAverage value: 44.4 MPa Grade Count:17
Flexural Modulus 2.76 - 7.60 GPaAverage value: 4.64 GPa Grade Count:27
Izod Impact, Notched 0.214 - 1.07 J/cmAverage value: 0.439 J/cm Grade Count:26
Izod Impact, Unnotched 1.60 - 5.34 J/cmAverage value: 2.76 J/cm Grade Count:7
Izod Impact, Notched (ISO) 1.90 - 1.90 kJ/m²
@Temperature -40.0 - -40.0 °C
Average value: 1.90 kJ/m² Grade Count:1
Charpy Impact Unnotched 0.800 - 0.800 J/cm²
@Temperature -20.0 - -20.0 °C
Average value: 0.800 J/cm² Grade Count:1
Charpy Impact, Notched 0.100 - 0.100 J/cm²
@Temperature -20.0 - -20.0 °C
Average value: 0.100 J/cm² Grade Count:1
Gardner Impact 0.300 - 2.26 JAverage value: 1.01 J Grade Count:8
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 101 - 149 °CAverage value: 129 °C Grade Count:25
Deflection Temperature at 1.8 MPa (264 psi) 62.8 - 113 °CAverage value: 85.6 °C Grade Count:22
Flammability, UL94 HBGrade Count:6
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 210 - 238 °CAverage value: 227 °C Grade Count:6
Melt Temperature 180 - 249 °CAverage value: 218 °C Grade Count:9
Mold Temperature 26.7 - 70.0 °CAverage value: 46.9 °C Grade Count:10
Drying Temperature 65.6 - 100 °CAverage value: 82.5 °C Grade Count:9
Moisture Content 0.0500 %Average value: 0.0500 % Grade Count:4
Injection Pressure 2.76 - 103 MPaAverage value: 33.1 MPa Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 30% Mica Filler
Overview of materials for Polypropylene with 40% Talc Filler
Overview of materials for Polypropylene, Extrusion Grade
Overview of materials for Polypropylene with 10% Mica Filler
Overview of materials for Polypropylene with 20% Mica Filler

O4769 / 78405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.