MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Virantage® VW-10700 RP, RFP, RSFP Polyethersulfone (PESU), Amorphous
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Amorphous, high-temperature, features reactive end groups to enhance solubility

Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial properties in epoxy thermosets. Their inherent toughness imparts damage tolerance to thermoset composites and excellent flexibility to coatings. Virantage® polymers also offer superior thermal and hydrolytic stability that delivers best-in-class hot-wet performance.

They are especially suitable for incorporation into advanced composite resin systems used to produce high-performance aerospace components and have been used successfully in a variety of thermosetting resin systems including epoxies, phenolics, and BMIs.

Virantage® VW-series polymers are available in a range of molecular weights: high (10200), medium (10300) and low (10700). A range of particle sizes are also available to meet formulators' specific needs.

All Virantage® PESU polymers are produced at Solvay's state-of-the-art, world-scale facility in Panoli, India under ISO 9001:2000 and ISO 14001:2004 certified quality management systems.

Typical Particle Size ~D90
- VW-10700RFP 75.0 µm
- VW-10700RP 500 µm
- VW-10700RSFP 45.0 µm

Markets/Uses: Composites / Advanced Composites / High-Temperature Tougheners

Applications: Aerospace Applications

Features: Amorphous; Good Thermal Stability; Good Toughness; High Heat Resistance; Hydrolytically Stable; Low Molecular Weight; Low Viscosity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 560 cP560 cPSolution Viscosity; ASTM D445
Molecular Weight 21000 g/mol21000 g/molAverage
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 216 °C421 °FASTM E1356
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
OH End Groups210 µeq/g
ProcessingCoating; Compounding
Residual Solvent(%)0.15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4618 / 280418

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.