MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® TG 460 sheet Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Rail glazing Makrolon® TG 460 sheet is a hard-coated polycarbonate product designed for high optical quality and exceptional durability. This 0.460 in. thick product meets stringent U.S. Federal Railroad Administration requirements for impact, ballistic, and flammability performance. State-of-the-art manufacturing and inspection processes provide low optical distortion and the advanced hard coat technology provides excellent abrasion resistance, chemical resistance, and long lasting outdoor weathering performance. This product is available in clear and a variety of standard and custom tints. Makrolon TG 460 is offered with a seven (7) year Limited Product Warranty against breakage for flat vertical applications.

Applications: Passenger rail car windows and other transportation glazing

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Ultimate 65.5 MPaASTM D638
Modulus of Elasticity 2.34 GPaASTM D638
Flexural Strength 93.1 MPaASTM D790
Compressive Strength 86.2 MPaASTM D695
Poissons Ratio 0.38ASTM E132
Izod Impact, Notched 16.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
ASTM D256
Impact Test >= 47.0 ft-lb
@Thickness 3.17 mm
ASTM D3763
Taber Abrasion, mg/1000 Cycles 2.0
@Load 0.500 kg
CS-10F Wheel; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.20e+16 ohm-cmASTM D257
Dielectric Constant 2.96
@Frequency 10 Hz
ASTM D 150
 3.17
@Frequency 60 Hz
ASTM D 150
Dielectric Strength 15.0 kV/mm
@Thickness 3.17 mm
ASTM D149
Dissipation Factor 0.00090
@Frequency 60 Hz
ASTM D150
 0.010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 10 secStainless Steel Strip Electrode; ASTM D495
 120 secTungsten Electrodes; ASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 37.5 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 142 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 84 %
@Thickness 5.99 mm
ASTM D1003
 
Descriptive Properties
Chemical ResistanceAcetone>24 Hrs
 Ammonia (10% concentration)>24 Hrs
 Antifreeze (50/50)>24 Hrs
 Benzene>24 Hrs
 Bleach (Clorox concentrated)>24 Hrs
 Chloroform>24 Hrs
 Denatured Alcohol>24 Hrs
 Di (2-ethylhexyl) phthalate>24 Hrs
 Diesel Oil>24 Hrs
 Hydrochloric Acid (20%)>24 Hrs
 Isopropyl Alcohol (IPA)>24 Hrs
 Kerosene>24 Hrs
 Methyl Alcohol>24 Hrs
 Methyl Butyl Ketone>24 Hrs
 Methyl Ethyl Ketone>24 Hrs
 Methylene Chloride>24 Hrs
 Naphthalene, 1-bromo->24 Hrs
 Nitric Acid (20%)>24 Hrs
 Potassium Hydroxide - Lye (10%)>24 Hrs
 Sodium Hydroxide (10%)>24 Hrs
 Sulfuric Acid (20%)>24 Hrs
 Toluene>24 Hrs
 Turpentine>24 Hrs
 Unleaded Gasoline (87 Octane)>24 Hrs
 Vinegar>24 Hrs
 Xylene>24 Hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® GP-V Prismatic sheet Polycarbonate
Covestro Makrolon® FI sheet Polycarbonate
Covestro Makrolon® BG sheet Polycarbonate
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer

PCOVEST0862 / 202645

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.