MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MarkeTech Carbon Nanofoam  (discontinued **)
Categories: Carbon; Ceramic; Aerogel

Material Notes: Electrically conductive carbon nanofoams possess many of the properties of traditional aerogel material. These materials are available in the form of monoliths, granules, powders and papers. They are synthetic, lightweight foams in which the solid matrix and pore spaces have nanometer-scale dimensions. Prepared by sol-gel methods, nanofoams typically have low density, continuous porosity, high surface area, and fine cell/pore sizes. The foams are also electrically conductive and have a high capacitance.

Carbon nanofoams are being used as lightweight, high temperature insulation, absorbents and coatings, specialty optics, and electrodes for water deionization cells, fuel cells, and other devices. Morphology examination by scanning electron microscope shows an open cell structure and continuous porosity. The particle size and pore spacing is a function of density and the polymerization chemistry used during the sol-gel process. Low density carbon nanofoams (~0.25 g/cm3) have the largest cell/pore size with particle diameters of up to 100 nm and pores at least 500 nm. High density carbon foams (abt. 0.8 g/cm3) have ultra fine particles and pores of less than 1000Å.

Data provided by the supplier, MarkeTech International.

MarkeTech International is no longer in business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.250 - 1.00 g/ccavailable range
Specific Surface Area 400 m²/gBET; at density = 0.8 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.010 - 0.040 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0890 W/m-K
 
Descriptive Properties
Average Pore Size0.7 nmat density = 0.8 g/cc
Capacitance30 F/gat density = 0.8 g/cc
ColorBlack
Gas Permeability1.47 x 10-10

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Silica Aerogel
MarkeTech Carbon Aerogel
MarkeTech Resorcinol Formaldehyde Aerogel
Graphite, Carbon, C
Vitreous Carbon (Glassy Carbon)

C5MTO3a / 375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.