MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Emerald Performance Materials Hypro™ 2000X162 CTB Carboxyl-Terminated Butadiene
Categories: Polymer; Thermoset

Material Notes: Chemical intermediate to incorporate polybutadiene into other resins.

Information provided by Emerald Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.907 g/cc0.907 g/cc
Viscosity 50000 cP50000 cP
Molecular Weight 4200 g/mol4200 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 2525[mgKOH/g]
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -77.0 °C-107 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 3.03.0
 
Descriptive Properties
Acrylonitrile0 percent
Carboxyl Equiv0.045 phr
Functionality1.9
Solubility Parameter8.14 cal/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Magnum™ 758HP ABS, High Heat, High Impact
Overview of materials for Nylon 6, Heat Stabilized
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance

PEMERA860 / 209688

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.