Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 5% Filler by Weight Additive: Heat Stabilizer and Impact Modifier Features: Heat Stabilized and Impact Modified Appearance: Black Information provided by TP Composites, Inc. |