MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mapal Plastics Maplon CFA-HK Polypropylene Sheet
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/cc
@Thickness 0.430 mm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 20.0 MPa
@Thickness 0.430 mm,
Temperature 23.0 °C
ASTM D638
 20.0 MPa
@Thickness 0.250 mm,
Temperature 23.0 °C
ASTM D638
Film Tensile Strength at Yield, TD 16.0 MPa
@Thickness 0.430 mm,
Temperature 23.0 °C
ASTM D638
 16.0 MPa
@Thickness 0.250 mm,
Temperature 23.0 °C
ASTM D638
Film Elongation at Yield, MD 16 %
@Thickness 0.250 mm,
Temperature 23.0 °C
ASTM D638
 18 %
@Thickness 0.430 mm,
Temperature 23.0 °C
ASTM D638
Film Elongation at Yield, TD 9.0 %
@Thickness 0.250 mm,
Temperature 23.0 °C
ASTM D638
 14 %
@Thickness 0.430 mm,
Temperature 23.0 °C
ASTM D638
Modulus of Elasticity 0.300 GPa
@Thickness 0.430 mm,
Temperature 23.0 °C
TD; ASTM D638
 0.350 GPa
@Thickness 0.250 mm,
Temperature 23.0 °C
TD; ASTM D638
 0.350 GPa
@Thickness 0.430 mm,
Temperature 23.0 °C
ASTM D638
 0.400 GPa
@Thickness 0.250 mm,
Temperature 23.0 °C
ASTM D638
Flexural Modulus 1278 MPa
@Thickness 3.20 mm,
Temperature 23.0 °C
Izod Impact, Notched 50.0 J/m
@Thickness 3.20 mm,
Temperature -20.0 °C
ASTM D256
 250 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+9 ohm
@Thickness 0.430 mm
ASTM D257
 1.00e+9 ohm
@Thickness 0.250 mm
ASTM D257
Dielectric Breakdown 15000 V
@Thickness 0.250 mm
ASTM D149
 20000 V
@Thickness 0.430 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 150 °C
@Thickness 0.430 mm
ASTM D1525
 150 °C
@Thickness 0.250 mm
ASTM D1525
Heat Distortion Temperature 85.0 °C
@Thickness 0.430 mm
ASTM 648
 85.0 °C
@Thickness 0.250 mm
ASTM 648
Flammability, UL94 V-0
@Thickness 0.430 mm
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOL GP-3152F General Purpose Polypropylene, 15% Mineral Fillers, High Impact, Flame Retardant
LG Chemical LUPOL GP-3154F General Purpose Polypropylene, 15% Mineral Fillers, High Modulus, Flame Retardant
Loxim 820 02T V0 Polypropylene Compound, 20% Talc Filled, Flame Retardant
Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant
Avient Maxxam™ FR PP FR 8-6 A NATURAL - ROHS Polypropylene

PMAPAL08 / 83619

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.