MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Honeywell Solstice® Propellant
Categories: Fluid

Material Notes: Solstice Propellant, is a new, nonflammable aerosol propellant that has an ultra-low global warming potential (GWP) and very low photochemical reactivity. Its full chemical name is trans- 1,3,3,3-tetrafluoroprop-1-ene, also known as HFO-1234ze. Its INCI name is tetrafluoropropene. The chemical structure is shown in Figure 1.

Molecular Formula: CHF=CHCF3

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccLiquid
 1.057 g/cc
@Temperature 54.0 °C
 1.069 g/cc
@Temperature 51.0 °C
 1.081 g/cc
@Temperature 48.0 °C
 1.092 g/cc
@Temperature 45.0 °C
 1.104 g/cc
@Temperature 42.0 °C
 1.1149 g/cc
@Temperature 39.0 °C
 1.123 g/cc
@Temperature 9.00 °C
 1.125 g/cc
@Temperature 36.0 °C
 1.131 g/cc
@Temperature 3.00 °C
 1.136 g/cc
@Temperature 33.0 °C
 1.146 g/cc
@Temperature 30.0 °C
 1.156 g/cc
@Temperature 27.0 °C
 1.166 g/cc
@Temperature 24.0 °C
 1.176 g/cc
@Temperature 21.0 °C
 1.185 g/cc
@Temperature 18.0 °C
 1.195 g/cc
@Temperature 15.0 °C
 1.204 g/cc
@Temperature 12.0 °C
 1.22 g/cc
@Temperature 6.00 °C
 1.24 g/cc
@Temperature 0.000 °C
 1.248 g/cc
@Temperature -3.00 °C
 1.257 g/cc
@Temperature -6.00 °C
 1.266 g/cc
@Temperature -9.00 °C
 1.27 g/cc
@Temperature -12.0 °C
 1.28 g/cc
@Temperature -15.0 °C
Molecular Weight 114 g/mol
Vapor Pressure 801.6 torr
@Temperature -17.8 °C
 899.8 torr
@Temperature -15.0 °C
 1005.9 torr
@Temperature -12.2 °C
 1127.4 torr
@Temperature -9.44 °C
 1261.8 torr
@Temperature -6.67 °C
 1401.5 torr
@Temperature -3.89 °C
 1556.6 torr
@Temperature -1.11 °C
 1727.3 torr
@Temperature 1.67 °C
 1908.3 torr
@Temperature 4.44 °C
 2099.6 torr
@Temperature 7.22 °C
 2550.2 torr
@Temperature 21.1 °C
 3706.9 torr
@Temperature 27.8 °C
 3736.9 torr
@Temperature 26.7 °C
 3766.4 torr
@Temperature 385 °C
 3795.4 torr
@Temperature 21.1 °C
 3824.3 torr
@Temperature 18.3 °C
 3852.2 torr
@Temperature 15.6 °C
 3880.2 torr
@Temperature 12.8 °C
 3907.6 torr
@Temperature 10.0 °C
 4628.5 torr
@Temperature 32.2 °C
 5006 torr
@Temperature 35.0 °C
 5409.4 torr
@Temperature 37.8 °C
 5838.6 torr
@Temperature 40.6 °C
 6288.5 torr
@Temperature 43.3 °C
 6769.5 torr
@Temperature 46.1 °C
 7271.1 torr
@Temperature 48.9 °C
 7500.6 torr
@Temperature 54.4 °C
 7803.8 torr
@Temperature 51.7 °C
 8367.5 torr
@Temperature 54.4 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 1.20 kV/in
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 84.0 BTU/lb
Boiling Point -2.20 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Sulfur Cure
Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A
DuPont Mobility and Materials Delrin® 500TL NC010 POM-SD
DuPont Mobility and Materials Delrin® 500AF POM-SF20
DuPont Mobility and Materials Delrin® 100ST BK602 POM-HI

PHONWL172 / 179717

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.