MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Yuyao Zhonga NR ABS, Heat Resistance
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: Heat resistance ABS offers good heat resistance, good impact, good processability, and good flammability after joined flame retardant agent. Heat resistance, heat-resistance flame retardant ABS is used for mirror frame, hair drier shells, electric cooker parts, main and vice automobile instrument panel, vent cover, steering wheel, cooling grid, loudhailer, microwave oven parts, air conditioner fan, luminaire.

Information provided by Yuyao Zhongfa Engineering Plastics CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 3.5 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100
Tensile Strength 42.0 MPaASTM D638
Elongation at Break 30 %ASTM D638
Flexural Strength 80.0 MPaASTM D790
Flexural Modulus 2000 MPaASTM D790
Charpy Impact Unnotched 20.0 kJ/m²ASTM D256
Charpy Impact, Notched 20.0 kJ/m²ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 225 °CInjection Temp
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 80.0 - 85.0 °C
Dry Time 2.00 - 3.00 hour
Injection Pressure 60.0 - 90.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PYUYZ038 / 281831

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.