MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2799 S X 118623 B Saturated Styrenic Block Copolymer, EMI/RFI Shielding
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.68 g/cc1.68 g/ccASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 555510 s delay; ASTM D 2240
Tensile Strength at Break 2.21 MPa
@Thickness 3.17 mm
320 psi
@Thickness 0.125 in
Break; Die C; 20 in/min (500 mm/min); ASTM D412
Tensile Stress at Strain 1.97 MPa
@Strain 100 %,
Thickness 3.17 mm
285 psi
@Strain 100 %,
Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
Elongation at Break 320 %
@Thickness 3.17 mm
320 %
@Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
Tear Strength 19.3 kN/m110 pliDie C; ASTM D 624
Compression Set  12 %
@Temperature 23.0 °C,
Time 79200 sec
12 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 64 %
@Temperature 70.0 °C,
Time 79200 sec
64 %
@Temperature 158 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.0 ohm-cm<= 1.0 ohm-cmASTM D 257
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 °C400 °F
Mold Temperature 21.1 - 60.0 °C70.0 - 140 °F
Drying Temperature 76.7 °C170 °F
Dry Time 2 - 3 hour2 - 3 hour
Moisture Content <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Premix Thermoplastics PRESEAL® TPE 5020
RTP Company EMI 2184  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 25%
RTP Company EMI 2183  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 20%
RTP Company EMI 2162 Polyetherimide (PEI); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1382  Polyphenylene Sulfide (PPS) Shielding - Nickel-Coated Carbon Fiber 15%

PQZWA12889 / 90740

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.