MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CLAL-MSX NICLAFOR® 1000 TDX Quenched/Cold Rolled, Drawn Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeability, good formability, long life duration. Meets environmental concern by not containing Beryllium, Cadmium nor Titanium.

Applications:

  • Electrotechnic
  • Electromechanic
  • Electronic
  • Connectic
  • Automotive
  • Domestic appliances
  • Spectacle industry
  • Turned parts.

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 250 - 320250 - 320
Tensile Strength, Ultimate 880 - 1000 MPa128000 - 145000 psi
Tensile Strength, Yield >= 800 MPa
@Strain 0.2 %
>= 116000 psi
@Strain 0.2 %
Elongation at Break >= 0.010 %>= 0.010 %A50 mm
Modulus of Elasticity 120 GPa17400 ksi
Modulus of Rigidity 50.0 GPa7250 ksiTorsion
Fatigue Strength 450 MPa
@# of Cycles 1.00e+7
65300 psi
@# of Cycles 1.00e+7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00001433 ohm-cm<= 0.00001433 ohm-cmprecipitation hardened (3h)
 <= 0.00001911 ohm-cm<= 0.00001911 ohm-cmquenched
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.25 µm/m-°C
@Temperature 20.0 - 200 °C
9.583 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 53.6 W/m-K372 BTU-in/hr-ft²-°F
Melting Point 968 - 1078 °C1770 - 1972 °F
Solidus 968 °C1770 °F
Liquidus 1078 °C1972 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 82.65 - 85.95 %82.65 - 85.95 %
Iron, Fe <= 0.50 %<= 0.50 %
Lead, Pb <= 0.030 %<= 0.030 %
Manganese, Mn 0.050 - 0.30 %0.050 - 0.30 %
Nickel, Ni 8.5 - 9.5 %8.5 - 9.5 %
Phosphorus, P <= 0.020 %<= 0.020 %
Tin, Sn 5.5 - 6.5 %5.5 - 6.5 %
Zinc, Zn <= 0.50 %<= 0.50 %
 
Descriptive Properties
Striction>50%Coef. Z

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Beryllium Copper Alloy 190 Strip; 1/2HM (TM02) Temper (UNS C17200)
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard
Beryllium Copper, UNS C17200, TM08 Temper Strip
Beryllium Copper, UNS C17200, TM06 Temper Strip

NCLAL073 / 160104

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.