MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Telcar® TL-1934A BLK 111 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccASTM D792
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83ASTM D2240
Tensile Strength at Break 2250 psiASTM D412
Elongation at Break 630 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.36
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.00010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -76.0 °FASTM D746
Oxygen Index 18 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 340 - 380 °F
Middle Barrel Temperature 350 - 390 °F
Front Barrel Temperature 360 - 400 °F
Nozzle Temperature 370 - 410 °F
Zone 1 330 - 370 °F
Zone 2 340 - 380 °F
Zone 3 350 - 390 °F
Zone 5 360 - 400 °F
Die Temperature 374 - 410 °F
Melt Temperature 370 - 410 °FProcessing Temperature
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer
Teknor Apex Medalist® MD-8431 Thermoplastic Elastomer
Teknor Apex Elexar® EL-8730A Thermoplastic Elastomer
Teknor Apex Elexar® EL-8452 Thermoplastic Elastomer
Teknor Apex ELEXAR® EL 8451 Thermoplastic Elastomer

PTEKNP421 / 129502

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.