MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aclo Accutech Polypropylene Homopolymer HP0339C30L1 Calcium Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Calcium Carbonate (CaCO3) Filler

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.113 g/ccASTM D792
Linear Mold Shrinkage 0.012 cm/cmMD; ASTM D955
Melt Flow 21 g/10 minASTM D1238
Ash 30 %ASTM D2584
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 86ASTM D785
Tensile Strength at Break 2180 psiASTM D638
Tensile Strength, Yield 3920 psiASTM D638
Elongation at Break 40 %ASTM D638
Elongation at Yield 5.0 %ASTM D638
Tensile Modulus 233000 psiASTM D638
Flexural Strength 5370 psiASTM D790
Flexural Modulus 290000 psiASTM D790
Izod Impact, Notched 0.750 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 226 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HH450MO Polypropylene
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating
Braskem H362-09RS Cast Film Polypropylene
Amco PRIMATOP PP CO 200 NB Impact Polypropylene Copolymer
Overview of materials for Polypropylene with 50% Glass Fiber Filler

PACLO141 / 22396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.