MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem Green PE SGM9450F Blow Film Extrusion and Cast Film Extrusion High Density Polyethylene
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Description: SGM9450F is a high-density polyethylene, developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tenacity and excellent resistance to impact characteristics. This resin has wide molar mass distribution that makes it easier to process. The minimum biobased content of this grade is 96%, determined according to ASTM D6866.

Application: Bags in general (like T-shirt bags, Handle Bags, Star Bags, others); Geomembranes.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.952 g/ccASTM D1505/D792
Thickness 12.5 microns
Melt Flow 0.33 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 9.3 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 590 %ASTM D882
Film Elongation at Break, TD 740 %ASTM D882
Elmendorf Tear Strength MD 58 ggF; ASTM D1922
Elmendorf Tear Strength TD 51 ggF; ASTM D1922
Dart Drop Test 245 gg/F50; ASTM D1709
Film Tensile Strength at Break, MD 85.0 MPaASTM D882
Film Tensile Strength at Break, TD 45.0 MPaASTM D882
Heat Seal Strength Initiation Temperature 125 °C
 
Descriptive Properties
Puncture Strength80 J/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem Green PE SGD4960 Blow Molded High Density Polyethylene
Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Braskem Green PE SLL5405S Blown Film Extrusion High Density Polyethylene
Braskem Green PE SBC818R50 Extrusion Coating Low Density Polyethylene
Braskem Green PE SBC818 Extrusion Coating Low Density Polyethylene

PBRAS700 / 109537

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.