Description: TIPELIN 7700M is a natural, high density polyethylene copolymer (with butene-1 as comonomer) grade. The product shows excellent mechanical properties and environmental stress crack resistance (ESCR). The grade contains antioxidant and acid scavenger. Applications: TIPELIN 7700M is recommended for non-pressure pipes and sheet manufacturing. (1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). Information provided by Molgroup Chemicals |