MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
303 Stainless Steel, annealed
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Short time tensile test

Key Words: T303, T 303, 303SS, 303 SS, AFNOR Z 10 CNF 18.09 (Fr), UNI X 10 CrNiS 18 09, SUS 303, SS14 2346 (Sweden), B.S. 303 S 21, UNS S30300, AMS 5640 (1), ASME SA194, ASME SA320, ASTM A194, ASTM A314, ASTM A320, ASTM A320, ASTM A473, ASTM A581, ASTM A582, MIL SPEC MIL-S-862, SAE J405 (30303), DIN 1.4305, X12CrNiS188, EN 58M, austenitic, ISO 683/13 17, 18-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 620 MPa
 140 MPa
@Temperature 870 °C
 205 MPa
@Temperature 760 °C
 310 MPa
@Temperature 650 °C
 380 MPa
@Temperature 540 °C
 420 MPa
@Temperature 425 °C
Tensile Strength, Yield 240 MPa
@Strain 0.2 %
 70.0 MPa
@Strain 0.2 %,
Temperature 870 °C
 145 MPa
@Strain 0.2 %,
Temperature 760 °C
 205 MPa
@Strain 0.2 %,
Temperature 650 °C
 235 MPa
@Strain 0.2 %,
Temperature 540 °C
 240 MPa
@Strain 0.2 %,
Temperature 425 °C
Elongation at Break 50 %in 50 mm
 30 %
@Temperature 650 °C
in 50 mm
 31 %
@Temperature 760 °C
in 50 mm
 34 %
@Temperature 870 °C
in 50 mm
 34 %
@Temperature 540 °C
in 50 mm
 35 %
@Temperature 425 °C
in 50 mm
Tensile Modulus 193 GPa
Poissons Ratio 0.25Calculated
Fatigue Strength 240 MPaannealed
 330 MPa25% hardened
Shear Modulus 77.2 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
Magnetic Permeability 1.008at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.2 µm/m-°C
@Temperature 0.000 - 100 °C
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.2 W/m-K
@Temperature 100 °C
 21.5 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1420 °C
Solidus 1400 °C
Liquidus 1420 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 18 %
Iron, Fe 69 %
Manganese, Mn <= 2.0 %
Molybdenum, Mo <= 0.60 %
Nickel, Ni 9.0 %
Phosphorus, P <= 0.20 %
Silicon, Si <= 1.0 %
Sulfur, S >= 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
303 Stainless Steel, annealed bar
303 Stainless Steel, cold drawn bar
302 Stainless Steel, annealed strip
AISI 303 Cast Stainless Steel, ASTM A582

MQ303A / 12656

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.