MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® Nature Range M79-LT Bio-derived Epoxy Matrix
Categories: Polymer; Renewable/Recycled Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® Nature Range NR-M79-LT is a hotmelt, thermosetting, low-exothermic epoxy resin matrix, specifically designed for prepreg applications at which short cure cycles below 100°C are required. NR-M79-LT can be used for manufacture of large industrial components, suitable for cure of thin and thick sections. NR-M79-LT exhibits a long out-life of 8 weeks at ambient conditions. NR-M79-LT is supplied as low tack resin matrix.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.20 g/cc0.0397 - 0.0434 lb/in³
Viscosity  1100 cP
@Temperature 95.0 °C
1100 cP
@Temperature 203 °F
@1°C/min
 1.00e+7 cP
@Temperature 25.0 °C
1.00e+7 cP
@Temperature 77.0 °F
@1°C/min
 1.00e+7 cP
@Temperature 120 °C
1.00e+7 cP
@Temperature 248 °F
@1°C/min
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 90.0 - 100 °C194 - 212 °FTypical cured, following a 130min cure @90°C
 100 - 110 °C212 - 230 °FOptimum cured, following a 120min cure @110°C
 
Processing PropertiesMetricEnglishComments
Cure Time  <= 60.0 min
@Temperature 110 °C
<= 1.00 hour
@Temperature 230 °F
time to 95% conversion; ISO 11357-5
 <= 60.0 min
@Temperature 120 °C
<= 1.00 hour
@Temperature 248 °F
time to 95% conversion; ISO 11357-5
 <= 75.0 min
@Temperature 100 °C
<= 1.25 hour
@Temperature 212 °F
time to 95% conversion; ISO 11357-5
 <= 130 min
@Temperature 90.0 °C
<= 2.17 hour
@Temperature 194 °F
time to 95% conversion; ISO 11357-5
 <= 240 min
@Temperature 80.0 °C
<= 4.00 hour
@Temperature 176 °F
time to 95% conversion; ISO 11357-5
 <= 360 min
@Temperature 75.0 °C
<= 6.00 hour
@Temperature 167 °F
time to 95% conversion; ISO 11357-5
 <= 480 min
@Temperature 70.0 °C
<= 8.00 hour
@Temperature 158 °F
time to 95% conversion; ISO 11357-5
Shelf Life  >= 0.750 Month
@Temperature 30.0 °C
>= 0.750 Month
@Temperature 86.0 °F
 >= 2.00 Month
@Temperature 23.0 °C
>= 2.00 Month
@Temperature 73.4 °F
 >= 6.00 Month
@Temperature 5.00 °C
>= 6.00 Month
@Temperature 41.0 °F
 >= 24.0 Month
@Temperature -18.0 °C
>= 24.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
ColorOff-White - Yellowish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9163 / 322319

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.