MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Pluracol® 4850 Slabstock HR & Molded Graft Polyol
Categories: Fluid

Material Notes: Description: Pluracol® 4850 polyol is a primary hydroxyl-terminated graft polyether triol containing approximately 32% solids of copolymerized styrene and acrylonitrile, utilizing a LVI inhibitor package. Pluracol 4850 can be used in combination with Pluracol 2100 to produce HR slabstock foams having a narrow spread in cross-sectional density and IFD properties and allows foam manufacturers to adjust the solids levels to specific formulations. Broad processing latitude permits the manufacture of a wide variety of high resilient foams. Pluracol 4850 polyol can also be used in molded foam applications.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.03 g/cc
@Temperature 40.0 °C
0.0372 lb/in³
@Temperature 104 °F
 1.04 g/cc
@Temperature 25.0 °C
0.0376 lb/in³
@Temperature 77.0 °F
Viscosity  1620 cP
@Temperature 40.0 °C
1620 cP
@Temperature 104 °F
 2950 cP
@Temperature 25.0 °C
2950 cP
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.16 J/g-°C0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K0.868 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %STI 3062
 
Descriptive Properties
ColorCreamy, Opaque Liquid
Hydroxyl Number23 - 26 mg KOH/gSTI 3007/3162

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Lupranate® M20SB Isocyanate
BASF Pluracol® 4600 Graft Slabstock Foam Polyol
BASF Lupranate® M20HB Isocyanate
BASF Lupranate® M20FB Isocyanate
BASF Lupranate® M20 Isocyanate

PBASG0792 / 132425

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.